Refine results
Thermally Conductive
Platinum
10:1
300,000 cP
0.79 W/(mK)
*22) 0.8 W/mK Low Viscosity, *3) Primed Lap Shear 205 psi (1.4 MPa), Low Temp
Platinum
122 g/minute
0.95 W/(mK)
Platinum
20:1
140 g/minute
0.64 W/(mK)
*22) 0.6 W/mK, Thin Bond Line
Platinum
10:1
900,000 cP
1.11 W/(mK)
Showing 11 to 14 of 14 entries